AWM 3135 Heat Resistant Silicone Rubber Wire

AWM 3135 Heat Resistant Silicone Rubber Wire
Request a Quote

Conductor: Bare, tinned copper
Insulator: Silicone rubber
Rated volt.: 600V
Test voltage: 2000V. 1min
Rated temp.: -60℃~ 200℃

Application
AWM 3135 heat resistant silicone rubber wires are used where high flexibility is required and in high temperature conditions. It is therefore a suitable connection cable for home electric appliance, high voltage machines like transformers, generators, motors, traction machines.

Technical Parameters
AWG
No.
Conductor Insulation Wire OD Resistance
Ω/KM
Max.
Size Structure OD Normal Normal Tolerance
mm² No./mm mm mm mm mm
26 0.128 7/0.16 0.48 0.76 2.00 ±0.10 148
24 0.205 7/0.20 0.6 0.76 2.15 ±0.10 93
22 0.324 7/0.25 0.75 0.76 2.3 ±0.15 55
20 0.519 7/0.31 10/0.26 0.96 0.69 2.4 0/-0.10 34.6
18 0.823 7/0.39 16/0.26 1.20 0.76 2.75 ±0.20 21.8
16 1.31 7/0.49 1.47 0.76 3.00 ±0.20 13.7
26/0.26 1.55 0.76 3.10
14 2.08 7/0.62 41/0.254 1.90 0.76 3.45 ±0.25 8.62
12 3.31 19/0.50 43/0.32 2.50 0.76 4.05 ±0.25 5.38
26 0.128 1/0.42 0.42 0.76 1.95 ±0.10 142
24 0.205 1/0.52 0.52 0.76 2.05 ±0.10 89
22 0.324 1/0.65 0.65 0.76 2.20 ±0.15 54.3
20 0.519 1/0.82 0.82 0.76 2.35 ±0.15 33.9
18 0.823 1/1.05 1.05 0.76 2.60 ±0.20 21.4
16 1.31 1/1.30 1.30 0.76 2.85 ±0.20 13.5

Mechanical Properties
Tensile strength: 3.45N/mm2 min.
Elongation at break of insulation: ≥100%
Min. bending radius: 6×OD
Standard: UL758, UL62, And UL1581
Meet with RoHS, REACH rules.

Characteristics
AWM 3135 heat resistant silicone rubber wire has very good flexibility and good performance of resistance to high temperature, range from -55℃ up to 200℃.
The use of silicone rubber, a high grade corona resistant insulation material, gives the cable excellent dielectric strength.