Ti 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo) Near alpha titanium alloy
Request a Quote
Features
- Ti 6-2-4-2 has good tensile strength and is commonly used in environments that get as hot as 538℃.
- It has excellent anti-fatigue and resistance to crack propagation
Chemical Analysis
% | Al | Sn | Zr | Mo | C | N | H | O | Si | Fe | Ti | Y |
Min | 5.5 | 1.8 | 3.6 | 1.8 | - | - | - | - | 0.06 | - | - | - |
Max | 6.75 | 2.2 | 4.4 | 2.2 | 0.05 | 0.05 | 0.015 | 0.1 | 0.1 | 0.25 | Balance | 0.005 |
Product Form
- Round bar
- Sheet & plate
- Welding wire
- Strip
Physical Properties
Density | Electrical Resistivity | Specific Heat Capacity | Thermal Conductivity | Mean Coefficient of Thermal Expansion | Melting Point |
4.54 g/cm3 | 1.85 - 1.90 µ½•m | 0.120 BTU/lb-°F, 0.502 J/g-°F | BTU-in/hr-ft2-°F (W/m-K): 48.0 (6.92) | µin/in-°F (µm/m-°C): 32.0 - 212 °F (0 - 100 °C): 4.28 (7.70) | 1588 - 1716 °C |
- Applications
- Compressor discs and blades
- Motorsport components
- Engine afterburner components