Chemical Composition in % for Grade 27KKH
C | Si | Mn | Ni | S | P | Cr | Co | Fe |
≤0.04 | ≤0.25 | 0.2 - 0.4 | ≤0.3 | ≤0.015 | ≤0.015 | 0.3 - 0.6 | 26.5 - 28 | Bal |
Mechanical Properties under Т=20oС for Grade 27KKH
Assortment | Tensile Strength | Yield Stress | Specific Elongation at Fracture |
- | MPa | MPa | % |
Band, GOST 10160-75 | 590 | 295 | 20 |
Band cold-worked, GOST 10160-75 | 1080 | 2 |
Physical Properties for Grade 27KKH
Test Temperature | Young Modulus 10-5 | Coefficient of Linear Expansion 106 | Density | Electrical Resistance 109 |
Grade | MPa | 1/Grade | kg/m3 | Ohm·m |
20 | 2.2 | 7980 | 200 | |
100 | 10.7 |